Optical constants of CARGILLE
Acrylic matching liquid
Wavelength:
µm
(0.31–1.55)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.47842+4.63182\text{×}10^{-3}λ^{-2}-8.63733\text{×}10^{-6}λ^{-4}$$Conditions
temperature: 298
Notes
25 °C
References
Data
Additional information
Properties of Acrylic matching liquid
density:
-
temperature: 298
value: 888
thermal_expansion:
-
temperature: 298
value: 0.0007
About Index-matching materials
An index-matching material is usually used to create an optical contact with minimum reflection between optical components.
Links