Optical constants of CARGILLE
Acrylic double matching liquid

Wavelength: µm
 (0.31–1.55)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.473749+6.5503120\text{×}10^{-3}λ^{-2}-1.2694420\text{×}10^{-5}λ^{-4}$$

Conditions

temperature: 298

Notes

25 °C

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of Acrylic double matching liquid

density:
  - 
    temperature: 298
    value: 1184
thermal_expansion:
  - 
    temperature: 298
    value: 0.00066

About Index-matching materials

An index-matching material is usually used to create an optical contact with minimum reflection between optical components.