Optical constants of CARGILLE
Fused silica matching liquid 50350
Wavelength:
µm
(0.225–1.55)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.446902+3.98963\text{×}10^{-3}λ^{-2}+3.757747\text{×}10^{-5}λ^{-4}$$Conditions
temperature: 298
Notes
25 °C.
References
Fused Silica Matching Liquid Code 50350 Data Sheet 30-NOV-17 (obtained from https://www.cargille.com)
Data
Additional information
Properties of Fused silica matching liquid 50350
density:
-
temperature: 298
value: 831
thermal_expansion:
-
temperature: 298
value: 0.0008
About Index-matching materials
An index-matching material is usually used to create an optical contact with minimum reflection between optical components.
Links