Optical constants of CARGILLE
Fused silica matching liquid 06350

Wavelength: µm
 (0.225–1.55)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.44719+3.83343\text{×}10^{-3}λ^{-2}+5.66134\text{×}10^{-5}λ^{-4}$$

Conditions

temperature: 298

Notes

25 °C.

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of Fused silica matching liquid 06350

density:
  - 
    temperature: 298
    value: 824
thermal_expansion:
  - 
    temperature: 298
    value: 0.0008

About Index-matching materials

An index-matching material is usually used to create an optical contact with minimum reflection between optical components.