RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CaYAlO4 (Calcium yttrium aluminate, CALYO)
Loiko et al. 2017: n(e) 0.35–2.1 µm

Wavelength: µm
 (0.35–2.1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=3.62156+\frac{0.03582}{λ^2-0.01920}-0.01298λ^{2}$$

Conditions

optical_component: e

Notes

Extraordinary optical constants (e); room temperature.

References

P. Loiko, P. Becker, L. Bohatý, C. Liebald, M. Peltz, S. Vernay, D. Rytz, J. M. Serres, X. Mateos, Y. Wang, X. Xu, J. Xu, A. Major, A. Baranov, U. Griebner, V. Petrov. Sellmeier equations, group velocity dispersion, and thermo-optic dispersion formulas for CaLnAlO4 (Ln = Y, Gd) laser host crystals. Opt. Lett., 42, 2275–2278 (2017)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Calcium yttrium aluminate

Calcium yttrium aluminate (CaYAlO4), abbreviated as CALYO, is an inorganic compound that adopts a monoclinic crystal structure. It is a multifunctional material that has garnered interest for its unique optical and photoluminescent properties. When doped with rare-earth ions like Ce3+ or Eu3+, CALYO demonstrates excellent photoluminescence and can serve as a useful host material for phosphors and solid-state lasers. Its moderate thermal stability and good mechanical properties also make it an attractive candidate for optical coatings and filters. Furthermore, its relatively wide bandgap and tunable refractive index make it a versatile material for photonic and optoelectronic applications, ranging from waveguides to photodetectors. CALYO can be synthesized through several methods including solid-state reactions and hydrothermal processes, allowing for precise control over its stoichiometry and crystal structure. Overall, the compound's distinctive properties make it a subject of active research and a material with potential for broad applications in the field of optics and photonics.

Other names and variations

  • CaYAlO4
  • CALYO