Optical constants of CaMoO4 (Calcium molybdate)
Bond 1965: n(o) 0.45–3.8 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{2.7840λ^2}{λ^2-0.1483^2}+\frac{1.2425λ^2}{λ^2-11.576^2}$$Conditions
optical_component: o
Notes
Ordinary optical constants (o). Room temperature.
References
- W. L. Bond.
Measurement of the refractive indices of several crystals.
J. Appl. Phys. 36, 1674-1677 (1965)
- Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009
- Ref. 2 provides a dispersion formula based on data from ref. 1
Data
Additional information
About Calcium molybdate
Calcium molybdate (CaMoO4) is an inorganic compound with a tetragonal crystal structure, widely used as a scintillator material for radiation detection applications. It exhibits a high density, good thermal stability, and strong resistance to radiation damage. When doped with rare-earth ions or other activators, CaMoO4 can demonstrate enhanced scintillation efficiency, making it particularly useful for gamma-ray and X-ray detection. Its optical properties, including a moderate refractive index and wide bandgap, have also led to its exploration as a host material for solid-state laser applications. The compound can be synthesized through various methods such as solid-state reaction, hydrothermal processes, or co-precipitation. It's worth noting that its non-hygroscopic nature allows for easy handling and long-term stability. Overall, the favorable physical and optical properties of calcium molybdate make it a material of interest in both scientific research and practical applications, particularly in the fields of radiation detection and optoelectronics.
Mineral: Powellite
Other names and variations
- CaMoO4
- Powellite