Optical constants of CaMoO4 (Calcium molybdate)
Bond 1965: n(e) 0.45–3.8 µm

Wavelength: µm
 (0.45–3.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.8045λ^2}{λ^2-0.1542^2}+\frac{1.0055λ^2}{λ^2-10.522^2}$$

Conditions

optical_component: e

Notes

Extraordinary optical constants (e). Room temperature.

References

  1. W. L. Bond. Measurement of the refractive indices of several crystals. J. Appl. Phys. 36, 1674-1677 (1965)
  2. Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009
  • Ref. 2 provides a dispersion formula based on data from ref. 1

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Calcium molybdate

Calcium molybdate (CaMoO4) is an inorganic compound with a tetragonal crystal structure, widely used as a scintillator material for radiation detection applications. It exhibits a high density, good thermal stability, and strong resistance to radiation damage. When doped with rare-earth ions or other activators, CaMoO4 can demonstrate enhanced scintillation efficiency, making it particularly useful for gamma-ray and X-ray detection. Its optical properties, including a moderate refractive index and wide bandgap, have also led to its exploration as a host material for solid-state laser applications. The compound can be synthesized through various methods such as solid-state reaction, hydrothermal processes, or co-precipitation. It's worth noting that its non-hygroscopic nature allows for easy handling and long-term stability. Overall, the favorable physical and optical properties of calcium molybdate make it a material of interest in both scientific research and practical applications, particularly in the fields of radiation detection and optoelectronics.

Mineral: Powellite

Other names and variations

  • CaMoO4
  • Powellite