Optical constants of CaF2 (Calcium fluoride)
Bosomworth 1967: k 45–1000 µm; 5 K
Complex refractive index (n+ik)
Derived optical constants
Conditions
temperature: 5
Notes
5 K
References
D. R. Bosomworth. Far-infrared optical properties of CaF2, SrF2, BaF2, and CdF2. Phys. Rev., 157, 709 (1967)
Data
Additional information
About Calcium fluoride
Calcium fluoride (CaF2) is an inorganic compound with a cubic crystal structure, exhibiting excellent optical transparency over a wide range of wavelengths, from ultraviolet to infrared. It has a low refractive index (approximately 1.43 at 589 nm) and minimal chromatic dispersion, making it a preferred material for lenses, optical windows, and other components in spectroscopy and high-resolution imaging systems. Due to its low solubility and chemical stability, it is highly resistant to weathering and corrosion, making it suitable for harsh environments. In the realm of laser applications, CaF2 is often used as an optical gain medium when doped with rare-earth ions such as ytterbium or erbium. The compound is synthesized through various methods, including precipitation from aqueous solutions and high-temperature reactions between calcium and fluorine gas. Its excellent optical, thermal, and chemical properties make calcium fluoride a material of considerable interest for a wide variety of optical and industrial applications.
Mineral: Fluorite (fluorspar)
Other names and variations
- CaF2
- Calcium difluoride
- Calcium(II) fluoride
- Fluorite
- Fluorspar
Links