RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CRYSTRAN - Optical materials
CsI - Caesium iodide

Wavelength: µm
 (0.238–50.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Caesium Iodide is grown by sealed ampoule Stockbarger techniques with ingots of approximately 70mm diameter. CsI is very soft and pliable. IUPAC International Union of Pure and applied Chemistry recommends the spelling as Cesium. UK Useage is Caesium.
REFERENCES:
(1) Handbook Optical Constants, ed Palik, V2, ISBN 0-12-544422-2
(2) Rodney, J.Opt.Soc.Am. V45, p987, 1955
(3) Combes et al, J.Opt.Soc.Am. V41, p215, 1951
(4) Kelly, Bureau of Mines Bulletin, No371, p51, 1934

References

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of CsI - Caesium iodide

density:
  - 
    value: 4510
thermal_dispersion:
  - 
    type: constant
    value: -9.93E-5
thermal_expansion:
  - 
    temperature: 293
    value: 4.83E-5
hardness:
  - 
    type: Knoop
    indenter_mass: 0.2
    value: 196000000
melting_point:
  - 
    value: 894
thermal_conductivity:
  - 
    temperature: 298
    value: 1.1
youngs_modulus:
  - 
    value: 5300000000
poissons_ratio:
  - 
    value: 0.214
solubility:
  - 
    temperature: 293
    value: 440