RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CR-39
Polymer: n 0.58929 µm

Wavelength: µm
 (0.58929–0.58929)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

20 °C

References

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About CR-39

Other names and variations

  • Allyl diglycol carbonate (ADC)
  • Columbia resin #39

Links