RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CH3NH3PbI3 (Methylammonium lead iodide, MAPbI3)
Leguy et al. 2015: n,k 0.249–0.789 µm

Wavelength: µm
 (0.2490–0.7890)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Single crystal CH3NH3PbI3; orientation unknown; room temperature; critical point model used for fit, 249 nm - 789 nm - fit not reliable for sub-bandgap region - see reference

References

A. M. A. Leguy, Y. Hu, M. Campoy-Quiles, M. I. Alonso, O. J. Weber, P. Azarhoosh, M. van Schilfgaarde, M. T. Weller, T Bein, J. Nelson, P. Docampo, P. R. F. Barnes. Reversible hydration of CH3NH3PbI3 in films, single crystals, and solar cells. Chem. Matter. 27, 3397-3407 (2015)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Methylammonium lead iodide

Methylammonium lead iodide (CH3NH3PbI3) is a prominent perovskite material used extensively in solar cell technology. It is renowned for its high photovoltaic efficiency due to its optimal band gap and strong light absorption capabilities. This compound typically forms a tetragonal crystalline structure that facilitates efficient charge transport, critical for its application in perovskite solar cells. Its optical properties, particularly its refractive index, are crucial for enhancing light-harvesting efficiency.

Despite its potential in renewable energy applications, CH3NH3PbI3 faces challenges related to environmental impact and stability, given its lead content and sensitivity to moisture and temperature.

Other names and variations

  • CH3NH3PbI3
  • MAPbI3

Links

About Perovskite