Optical constants of (C8H8)n-(C3H3N)m (Styrene-acrylonitrile, SAN)
Sultanova et al. 2009: n 0.4368–1.052 µm
Wavelength:
µm
(0.4368–1.052)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.3787λ^2}{λ^2-0.017842}$$Conditions
temperature: 293
Notes
20 °C
References
N. Sultanova, S. Kasarova and I. Nikolov. Dispersion properties of optical polymers, Acta Physica Polonica A 116, 585-587 (2009)
(fit of the experimental data with the Sellmeier dispersion formula: Mikhail Polyanskiy)
Data
Additional information
About Styrene-acrylonitrile
Other names and variations
- SAN
- C8H8)n-(C3H3N)m
- Styrene-acrylonitrile resin
- Styrene-acrylonitrile copolymer
Links