Optical constants of Bombyx mori (silkworm) silk
Perotto et al. 2017: Native fibroin film; n 0.3–1.7 µm

Wavelength: µm
 (0.3–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.551+0.0026λ^{-2}+2.4\text{×}10^{-4}λ^{-4}$$

Notes

Native Bombyx mori (silkworm) fibroin film

References

G. Perotto, Y. Zhang, D. Naskar, N. Patel, D. L. Kaplan, S. C. Kundu, F. G. Omenetto. The optical properties of regenerated silk fibroin films obtained from different sources. Appl. Phys. Lett. 111, 103702 (2017)