RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Bombyx mori (silkworm) silk
Bucciarelli et al. 2018: Photocrosslinkable sericin film, crosslinked; n 0.4–1.5 µm

Wavelength: µm
 (0.4–1.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.524+6\text{×}10^{-3}λ^{-2}+4\text{×}10^{-4}λ^{-4}$$

Notes

Photocrosslinkable sericin film. Formed using formic acid. Crosslinked.

References

A. Bucciarelli, V. Mulloni, D.Maniglio, R. K. Pal, V. K. Yadavalli, A. Motta, A. Quarant. A comparative study of the refractive index of silk protein thin films towards biomaterial based optical devices. Opt. Mater. 78, 407-414 (2018)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Silk