RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of BiFeO3 (Bismuth ferrite, BFO)
Kumar et al. 2008: n 0.197–1.67 µm, k 0.197–0.576 µm

Wavelength: µm
 (0.19706–1.6693)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 273

Notes

25 nm BiFeO3 film grown on (100)SrTiO3 substrate.

References

A. Kumar, R. C. Rai, N. J. Podraza, S. Denev, M. Ramirez, Y.-H. Chu, L. W. Martin, J. Ihlefeld, T. Heeg, J. Schubert, D. G. Schlom, J. Orenstein, R. Ramesh, R. W. Collins, J. L. Musfeldt, V. Gopalan. Linear and nonlinear optical properties of BiFeO3. Appl. Phys. Lett. 92, 121915 (2008) (Numerical data kindly provided by Ryan Haislmaier and Venkatraman Gopalan)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Bismuth ferrite

BiFeO3, commonly known as bismuth ferrite (BFO), is a multiferroic material that exhibits both ferroelectric and antiferromagnetic properties. In the realm of optics and optoelectronics, BFO has garnered interest for its potential in creating multifunctional devices, leveraging its coupled electric and magnetic order parameters. It shows promise for applications in photovoltaics, data storage, and spintronic devices due to its strong magnetoelectric coupling. The material possesses a distorted perovskite structure, which gives rise to its unique properties. Various methods, such as sol-gel, chemical vapor deposition (CVD), and pulsed laser deposition (PLD), can be used to synthesize high-quality BFO films. The material has also been doped with elements like lanthanum and titanium to enhance its functional properties or to adjust its bandgap for specific applications. One of the challenges with BFO is its relatively low Curie temperature and weak ferromagnetism at room temperature. Nonetheless, the ability to control both electric and magnetic properties by external fields makes BFO a subject of intensive research for future optoelectronic devices and sensors.

Other names and variations

  • BiFeO3
  • BFO

Links