Optical constants of Bi2Se3 (Bismuth selenide)
Ermolaev et al. 2023: CVD film; n,k 0.290–3.30 µm

Wavelength: µm
 (0.290–3.300)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

substrate: Si/SiO2

Notes

Bi2Se3 CVD film.

References

G. A. Ermolaev, I. S. Vyslanko, A. P. Tselin, M. A. El-Sayed, M. K. Tatmyshevskiy, A. S. Slavich, D. I. Yakubovsky, M. S. Mironov, A. B. Mazitov, A. Eghbali, D. A. Panova, R. I. Romanov, A. M. Markeev, I. A. Kruglov, S. M. Novikov, A. A. Vyshnevyy, A. V. Arsenin, V. S. Volkov. Broadband Optical Properties of Bi2Se3. Nanomater., 13, 1460 (2023) (Numerical data kindly provided by Georgy Ermolaev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Bismuth selenide

Bi2Se3, or bismuth selenide, is a layered compound with a rhombohedral crystal structure that has gained significant attention for its topological insulator properties. This material exhibits unique electronic states on its surface, while behaving as an insulator in its bulk. In the realm of optics, Bi2Se3 has shown promise for applications in photodetectors, modulators, and even as a platform for exploring exotic quantum phenomena. It has a high refractive index and exhibits strong optical anisotropy due to its layered crystal structure. Bi2Se3 also has a narrow bandgap and shows strong photoresponse across a broad spectrum, making it suitable for infrared applications. While the material can be synthesized through methods such as Bridgman-Stockbarger and chemical vapor deposition (CVD), it is somewhat sensitive to environmental conditions and may require protective coatings to maintain its properties. Overall, Bi2Se3 is a fascinating material that has captivated researchers for its intriguing electronic and optical characteristics, holding promise for future applications in optoelectronics and quantum computing.