RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of BaF2 (Barium fluoride)
Bosomworth 1967: n,k 56.5–1000 µm; 80 K

Wavelength: µm
 (56–1000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=\frac{6.56λ^{2}}{λ^2-52.910^{2}}+\frac{-6038.5}{λ^2-52.910^{2}}$$

Conditions

temperature: 80

Notes

80 K

References

D. R. Bosomworth. Far-infrared optical properties of CaF2, SrF2, BaF2, and CdF2. Phys. Rev., 157, 709 (1967)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Barium fluoride

BaF2, or barium fluoride, is a crystal that offers a wide transmission range, spanning from the ultraviolet into the mid-infrared regions. This material is commonly used in specialized optical applications such as scintillators in high-energy physics experiments, and as windows and lenses in infrared spectroscopy systems. It possesses a relatively low refractive index and high resistance to radiation damage, which makes it especially useful in extreme conditions. Additionally, BaF2 has fast scintillation response times, making it advantageous in fast-timing applications. One drawback, however, is that the crystal is hygroscopic, making it sensitive to moisture and requiring proper storage and handling to maintain its optical properties. It also has a lower resistance to thermal and mechanical shock compared to other fluoride crystals, which can be a consideration depending on the intended application. Despite these limitations, BaF2 remains a highly valuable material for specialized optical and photonic applications, owing to its broad transmission range and resilience to high-energy radiation.

Other names and variations

  • BaF2
  • Barium difluoride
  • Barium(II) fluoride

Links