Optical constants of BaF2 (Barium fluoride)
Bosomworth 1967: k 71.5–1000 µm; 200 K
Complex refractive index (n+ik)
Derived optical constants
Conditions
temperature: 200
Notes
200 K
References
D. R. Bosomworth. Far-infrared optical properties of CaF2, SrF2, BaF2, and CdF2. Phys. Rev., 157, 709 (1967)
Data
Additional information
About Barium fluoride
BaF2, or barium fluoride, is a crystal that offers a wide transmission range, spanning from the ultraviolet into the mid-infrared regions. This material is commonly used in specialized optical applications such as scintillators in high-energy physics experiments, and as windows and lenses in infrared spectroscopy systems. It possesses a relatively low refractive index and high resistance to radiation damage, which makes it especially useful in extreme conditions. Additionally, BaF2 has fast scintillation response times, making it advantageous in fast-timing applications. One drawback, however, is that the crystal is hygroscopic, making it sensitive to moisture and requiring proper storage and handling to maintain its optical properties. It also has a lower resistance to thermal and mechanical shock compared to other fluoride crystals, which can be a consideration depending on the intended application. Despite these limitations, BaF2 remains a highly valuable material for specialized optical and photonic applications, owing to its broad transmission range and resilience to high-energy radiation.
Other names and variations
- BaF2
- Barium difluoride
- Barium(II) fluoride
Links