RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Au-Ag (Gold-silver alloy)
Rioux et al. 2014: n,k 0.27–1.2 µm; 100% Au

Wavelength: µm
 (0.270–1.200)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

100% Au, 0% Ag. Model fitted on ellipsometric measurements on five different AuAg alloy thin film compositions; Thin film compositions: Au, Au:Ag 2:1, Au:Ag 1:1, Au:Ag 1:2, Ag; Film thickness: 80 nm

References

D. Rioux, S. Vallières, S. Besner, P. Muñoz, E. Mazur, M. Meunier. An analytic model for the dielectric function of Au, Ag, and their alloys. Adv. Opt. Mater. 2, 176-182 (2014) (See Supporting information for MATLAB model)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Electrum

Electrum, or green gold, is a naturally occurring alloy of gold and silver with trace amounts of copper and other metals.

Other names and variations

  • Green gold
  • Gold-silver alloy
  • Au-Ag

Links