Optical constants of Antheraea mylitta silk
Perotto et al. 2017: Fibroin film; n 0.3–1.695 µm
Wavelength:
µm
(0.3–1.695)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.5204+0.0036λ^{-2}+2.9\text{×}10^{-4}λ^{-4}$$Notes
Antheraea mylitta fibroin film
References
G. Perotto, Y. Zhang, D. Naskar, N. Patel, D. L. Kaplan, S. C. Kundu, F. G. Omenetto. The optical properties of regenerated silk fibroin films obtained from different sources. Appl. Phys. Lett. 111, 103702 (2017)