Optical constants of Antheraea assamensis silk
Perotto et al. 2017: Fibroin film; n 0.3–1.695 µm

Wavelength: µm
 (0.3–1.695)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.504+0.0047λ^{-2}+1.2\text{×}10^{-4}λ^{-4}$$

Notes

Antheraea assamensis fibroin film

References

G. Perotto, Y. Zhang, D. Naskar, N. Patel, D. L. Kaplan, S. C. Kundu, F. G. Omenetto. The optical properties of regenerated silk fibroin films obtained from different sources. Appl. Phys. Lett. 111, 103702 (2017)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]