RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlSb-GaSb (Aluminium gallium antimonide, AlGaSb)
Ferrini et al. 1998: n,k 0.207–2.480 µm; 0% Al

Wavelength: µm
 (0.207–2.480)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

AlxGa1−xSb, x = 0 (GaAs). Thin film grown by molecular beam epitaxy on a GaSb substrate.

References

R. Ferrini, M. Patrini, S. Franchi. Optical functions from 0.02 to 6 eV of AlxGa1−xSb/GaSb epitaxial layers. J. Appl Phys. 84, 4517-4524 (1998)