RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlSb (Aluminium antimonide)
Zollner et al. 1989: n,k 0.214–0.886 µm

Wavelength: µm
 (0.2138–0.8856)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

300 K

References

S. Zollner, C. Lin, E. Schönherr, A. Böhringer, M. Cardona. The dielectric function of AlSb from 1.4 to 5.8 eV determined by spectroscopic ellipsometry. J. Appl. Phys. 66, 383-387 (1989)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium antimonide

AlSb, or aluminum antimonide, is a III-V semiconductor compound with a zincblende crystal structure. It has a direct bandgap of approximately 1.6 eV at room temperature and is known for its high electron mobility, which makes it useful in high-frequency and high-speed electronic applications. AlSb is often utilized in heterostructures with other III-V materials, such as GaSb and InAs, to create devices like high-electron-mobility transistors (HEMTs) and infrared photodetectors. The material has a relatively low effective mass of electrons, which contributes to its high electron mobility and thereby makes it desirable for applications requiring rapid electron transport. AlSb is also of interest for thermophotovoltaic applications, given its narrow bandgap energy, which allows for efficient absorption of infrared radiation. However, the material poses challenges in terms of crystal growth and fabrication due to its sensitivity to defects and impurities. Additionally, antimonide-based materials like AlSb require stringent safety protocols due to the toxicity of antimony. Despite these challenges, AlSb continues to be a material of significant research interest, offering a combination of electrical and optical properties that are attractive for next-generation electronic and optoelectronic devices.

Other names and variations

  • AlSb

Links