RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlN-Al2O3 (Aluminium oxynitride, ALON)
Hartnett et al. 1998: 7.17 at.% N; n,k 0.24–5.6 µm

Wavelength: µm
 (0.24–5.6)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Nitrogen content: 7.17 at.%

References

T. M. Hartnett, S. D Bernstein, E. A Maguire, R. W Tustison. Optical properties of ALON (aluminum oxynitride). IR Phys. Technol, 39, 203-211 (1998)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium oxynitride

Other names and variations

  • AlON
  • ALON

Links