RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Perner et al. 2023: n 2.0–7.1 µm; 0% Al

Wavelength: µm
 (2–7.1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{9.705183027405873λ^2}{λ^2-0.38586135365339097^2}$$

Conditions

temperature: 295

Notes

Pure GaAs (interpolation for other alloy ratios possible). Relative standard uncertainty ≤3.3×10-4 over whole range. Optical measurements at 2.21 mbar and 22 °C.

References

L. W. Perner, G.-W. Truong, D. Follman, M. Prinz, G. Winkler, S. Puchegger, G. D. Cole, O. H. Heckl. Simultaneous measurement of mid-infrared refractive indices in thin-film heterostructures: Methodology and results for GaAs/AlGaAs. Phys. Rev. Res. 5, 033048 (2023) (Data kindly provided by the authors)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium gallium arsenide

Other names and variations

  • AlGaAs
  • Aluminum gallium arsenide

Links