Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Papatryfonos et al. 2021: n,k 0.260–1.88 µm; 45.2% Al
Wavelength:
µm
(0.26049–1.87868)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
AlxGa1-xAs; x = 0.452
References
K. Papatryfonos, T. Angelova, A. Brimont, B. Reid, S. Guldin, P. R. Smith, M. Tang, K. Li, A. J. Seeds, H. Liu, D. R. Selviah. Refractive indices of MBE-grown AlxGa1-xAs ternary alloys in the transparent wavelength region. AIP Adv. 11, 025327 (2021) (Numerical data kindly provided by Konstantinos Papatryfonos)
Data
Additional information
About Aluminium gallium arsenide
Other names and variations
- AlGaAs
- Aluminum gallium arsenide
Links