RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Papatryfonos et al. 2021: n,k 0.260–1.88 µm; 34.2% Al

Wavelength: µm
 (0.26049–1.87868)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

AlxGa1-xAs; x = 0.342

References

K. Papatryfonos, T. Angelova, A. Brimont, B. Reid, S. Guldin, P. R. Smith, M. Tang, K. Li, A. J. Seeds, H. Liu, D. R. Selviah. Refractive indices of MBE-grown AlxGa1-xAs ternary alloys in the transparent wavelength region. AIP Adv. 11, 025327 (2021) (Numerical data kindly provided by Konstantinos Papatryfonos)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium gallium arsenide

Other names and variations

  • AlGaAs
  • Aluminum gallium arsenide

Links