Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Gadras et al. 2025: n,k 0.450–1.40 µm; 53% Al, 600 °C

Wavelength: µm
 (4.502291e-01–1.399642e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 873

Notes

AlxGa1-xAs; x=0.53; 600 °C

References

P. Gadras, L. Bourdon, A. Fées, K. Ben Saddik, A. Guilhem, A. Arnoult. Optical refractive index measurements of AlGaAs at high temperature for fully automated molecular beam epitaxy growth of Bragg mirrors. J. Phys. D: Appl. Phys. 58, 0022-3727 (2025) (Numerical data kindly provided by Pierre Gadras)