Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Gadras et al. 2025: n,k 0.450–1.40 µm; 32% Al, 600 °C
Wavelength:
µm
(4.502291e-01–1.399642e+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 873
Notes
AlxGa1-xAs; x=0.32; 600 °C
References
P. Gadras, L. Bourdon, A. Fées, K. Ben Saddik, A. Guilhem, A. Arnoult. Optical refractive index measurements of AlGaAs at high temperature for fully automated molecular beam epitaxy growth of Bragg mirrors. J. Phys. D: Appl. Phys. 58, 0022-3727 (2025) (Numerical data kindly provided by Pierre Gadras)
Data
Additional information
About Aluminium gallium arsenide
Other names and variations
- AlGaAs
- Aluminum gallium arsenide
Links