RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Aspnes et al. 1986: n,k 0.207–0.827 µm; 59.0% Al

Wavelength: µm
 (0.2066–0.8266)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

AlxGa1-xAs; x = 0.590

References

D. E. Aspnes, S. M. Kelso, R. A. Logan, R. Bhat. Optical properties of AlxGa1-xAs. J. Appl. Phys. 60, 754-767 (1986)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium gallium arsenide

Other names and variations

  • AlGaAs
  • Aluminum gallium arsenide

Links