RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Adachi 1989: n,k 0.207–12.4 µm; 70.0% Al

Wavelength: µm
 (2.0664e-01–1.2398e+01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

AlxGa1-xAs; x=0.700

References

S. Adachi. Optical dispersion relations for GaP, GaAs, GaSb, InP, InAs, InSb, AlxGa1−xAs, and In1−xGaxAsyP1−y. J. Appl. Phys. 66, 6030-6040 (1989)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium gallium arsenide

Other names and variations

  • AlGaAs
  • Aluminum gallium arsenide

Links