Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Adachi 1989: n,k 0.207–12.4 µm; 31.5% Al
Wavelength:
µm
(2.0664e-01–1.2398e+01)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
AlxGa1-xAs; x=0.315
References
S. Adachi.
Optical dispersion relations for GaP, GaAs, GaSb, InP, InAs, InSb, AlxGa1−xAs, and In1−xGaxAsyP1−y.
J. Appl. Phys. 66, 6030-6040 (1989)
[Calculation script (Python)]
Data
Additional information
About Aluminium gallium arsenide
Other names and variations
- AlGaAs
- Aluminum gallium arsenide
Links