Optical constants of Al:ZnO (Aluminium-doped zinc oxide, AZO)
Treharne et al. 2011: n,k 0.3–0.9 µm
Wavelength:
µm
(0.300–0.900)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
An Al doped ZnO film (approx 2% wt. Al) was deposited on to a soda-lime glass substrate using RF magnetron sputtering. The resultant film had a resistivity of 4.7x10-4 Ω·cm. A variable-angle ellipsometer was used to take amplitude and phase change measurements. The refractive index and extinction coefficient was extracted from a multi-oscillator model fit to the ellipsometry data, as a function of wavelength, from 300 to 900 nm
References
R. E. Treharne, A. Seymour-Pierce, K. Durose, K. Hutchings, S. Roncallo, D. Lane. Optical design and fabrication of fully sputtered CdTe/CdS solar cells. J. Phys: Conf. Ser. 286, 012038, (2011) (Numerical data kindly provided by Dr. Robert Treharne)
Data
Additional information
About Aluminium-doped zinc oxide
Other names and variations
- AZO
- Al:ZnO
Links