Optical constants of Al:ZnO (Aluminium-doped zinc oxide, AZO)
Shkondin et al. 2017: n,k 2–20 µm

Wavelength: µm
 (2.00–20.00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Nanopillar.

References

E. Shkondin, O. Takayama, M. E. Aryaee Panah, P. Liu, P. V. Larsen, M. D. Mar, F. Jensen, A. V. Lavrinenko. Large-scale high aspect ratio Al-doped ZnO nanopillars arrays as anisotropic metamaterials. Opt. Mater. Express 7, 1606-1627 (2017) (Numerical data kindly provided by Osamu Takayama)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Aluminium-doped zinc oxide

Other names and variations

  • AZO
  • Al:ZnO

Links