Optical constants of AgGaS2-AgInS2
Kato et al. 2021: n(o) 0.565–10.6 µm
Wavelength:
µm
(0.565–10.6)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=11.15176+\frac{0.23052}{λ^2-0.07319}+\frac{11918.07}{λ^2-2224.38}$$Conditions
optical_component: o
Notes
AgGa0.86In0.14S2. Ordinary optical constants (o). Room temperature.
References
K. Kato, S. Banerjee, N. Uemura. Phase-matching properties of AgGa0.86In0.14S2 for three-wave interactions in the 0.615−10.5910 μm spectral range. Opt. Mater. Express, 11, 2800–2805 (2021)