RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of AgGaS2-AgInS2
Kato et al. 2021: n(e) 0.565–10.6 µm

Wavelength: µm
 (0.565–10.6)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=10.62054+\frac{0.22283}{λ^2-0.09609}+\frac{10591.78}{λ^2-2084.70}$$

Conditions

optical_component: e

Notes

AgGa0.86In0.14S2. Extraordinary optical constants (e). Room temperature.

References

K. Kato, S. Banerjee, N. Uemura. Phase-matching properties of AgGa0.86In0.14S2 for three-wave interactions in the 0.615−10.5910 μm spectral range. Opt. Mater. Express, 11, 2800–2805 (2021)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About AgGaS2-AgInS2