RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Ag (Silver)
Windt et al. 1988: n,k 0.0024–0.122 µm

Wavelength: µm
 (0.00236–0.12157)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Optical constants are derived from reflectance vs angle of incidence measurements using a nonlinear least-squares curve-fitting technique based on the χ2 test

References

D. L. Windt, W. C. Cash, M. Scott, P. Arendt, B. Newnam, R. F. Fisher, A. B. Swartzlander. Optical constants for thin films of Ti, Zr, Nb, Mo, Ru, Rh, Pd, Ag, Hf, Ta, W, Re, Ir, Os, Pt, and Au from 24 Å to 1216 Å. Appl. Opt. 27, 246-278 (1988)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Silver

Silver (Ag) is a highly reflective metal known for its excellent electrical and thermal conductivity, making it a material of interest in a variety of optical and electronic applications. In the realm of optics, silver is frequently used as a coating material for mirrors due to its high reflectivity across a broad range of wavelengths, from ultraviolet to infrared. Additionally, silver nanoparticles are employed in plasmonic devices, enhancing light-matter interactions at the nanoscale. While the metal is highly stable under most conditions, it is susceptible to tarnishing in the presence of sulfur compounds, which can diminish its optical performance over time. Silver's unique combination of properties, including its unparalleled reflectivity and high electrical conductivity, makes it a versatile material in the field of optics and photonics. Note that its refractive index can vary depending on the form in which it is used, such as bulk silver, thin films, or nanoparticles, making it crucial to consult specific data for particular applications.

Other names and variations

  • Ag

Links