Optical constants of Ag (Silver)
Choi et al. 2020: n,k 1.23–6.99 µm
Complex refractive index (n+ik)
Derived optical constants
Notes
Epitaxially grown, atomically smooth, single crystalline thick Ag film. Room temperature.
References
J. Choi, F. Cheng, J. W. Cleary, L. Sun, C. K. Dass, J. R. Hendrickson, C.-Y. Wang, S. Gwo, C.-K. Shih, X. Li. Optical dielectric constants of single crystalline silver films in the long wavelength range. Opt. Mater. Express 10, 693-703 (2020) (See supplementary materials)
Data
Additional information
About Silver
Silver (Ag) is a highly reflective metal known for its excellent electrical and thermal conductivity, making it a material of interest in a variety of optical and electronic applications. In the realm of optics, silver is frequently used as a coating material for mirrors due to its high reflectivity across a broad range of wavelengths, from ultraviolet to infrared. Additionally, silver nanoparticles are employed in plasmonic devices, enhancing light-matter interactions at the nanoscale. While the metal is highly stable under most conditions, it is susceptible to tarnishing in the presence of sulfur compounds, which can diminish its optical performance over time. Silver's unique combination of properties, including its unparalleled reflectivity and high electrical conductivity, makes it a versatile material in the field of optics and photonics. Note that its refractive index can vary depending on the form in which it is used, such as bulk silver, thin films, or nanoparticles, making it crucial to consult specific data for particular applications.
Other names and variations
- Ag
Links