Optical constants of Amorphous Materials - Infrared glass (AMTIR)
AMTIR-6

Wavelength: µm
 (0.6439–8.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

References

Amorphous Materials AMTIR-6 Information (2012) - downloaded 2014-01-11

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information