Optical constants of Amorphous Materials - Infrared glass (AMTIR)
AMTIR-2

Wavelength: µm
 (1–13)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{4.9948719λ^2}{λ^2-0.24164^2}+\frac{0.1207152λ^2}{λ^2-19^2}+\frac{1.7123685λ^2}{λ^2-0.48328^2}$$

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]