Optical constants of 5PCH (4-trans-pentylcyclohexylcyanobenzene)
Wu et al. 1993: n(o) 0.4–0.8 µm; 45.4 °C
Wavelength:
µm
(0.4–0.8)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n-1=0.3849+\frac{1.5133}{25.0000-λ^{-2}}+\frac{0.5432}{18.1077-λ^{-2}}$$Conditions
temperature: 318.55 optical_component: o
Notes
45.4 °C. Ordinary optical constants (o).
References
S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)
Data
Additional information
About Liquid crystals
Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.
Links