Optical constants of 5PCH (4-trans-pentylcyclohexylcyanobenzene)
Wu et al. 1993: n(o) 0.4–0.8 µm; 34.8 °C

Wavelength: µm
 (0.4–0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=0.3866+\frac{1.4900}{25.0000-λ^{-2}}+\frac{0.5300}{18.1077-λ^{-2}}$$

Conditions

temperature: 307.95
optical_component: o

Notes

34.8 °C. Ordinary optical constants (o).

References

S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)