Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Wu et al. 1993: n(o) 0.4–0.8 µm; 32.6 °C

Wavelength: µm
 (0.4–0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=0.4257+\frac{1.4135}{22.6757-λ^{-2}}+\frac{0.5272}{12.5748-λ^{-2}}$$

Conditions

temperature: 305.75
optical_component: o

Notes

32.6 °C. Ordinary optical constants (o).

References

S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Liquid crystals

Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.