Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Wu et al. 1993: n(e) 0.4–0.8 µm; 27.2 °C

Wavelength: µm
 (0.4–0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=0.4603+\frac{2.0874}{22.6757-λ^{-2}}+\frac{1.3544}{12.5748-λ^{-2}}$$

Conditions

temperature: 300.35
optical_component: e

Notes

29.9 °C. Extraordinary optical constants (e).

References

S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)