Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Tkachenko et al. 2006: n(o) 0.532–1.7 µm
Wavelength:
µm
(0.532–1.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.50849+0.00774λ^{-2}+0.00040λ^{-4}$$Conditions
optical_component: o
Notes
Ordinary optical constants (o).
References
V. Tkachenko, G. Abbate, A. Marino, F. Vita, M. Giocondo, A. Mazzulla, F. Ciuchi, L. De Stefano. Nematic liquid crystal optical dispersion in the visible-near infrared range. Mol. Cryst. Liq. Cryst. 454, 263/[665]-271/[673] (2006)
Data
Additional information
About Liquid crystals
Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.
Links