Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Tkachenko et al. 2006: n(e) 0.532–1.7 µm

Wavelength: µm
 (0.532–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.65535+0.01355λ^{-2}+0.00153λ^{-4}$$

Conditions

optical_component: e

Notes

Extraordinary optical constants (e).

References

V. Tkachenko, G. Abbate, A. Marino, F. Vita, M. Giocondo, A. Mazzulla, F. Ciuchi, L. De Stefano. Nematic liquid crystal optical dispersion in the visible-near infrared range, Mol. Cryst. Liq. Cryst. 454, 263/[665]-271/[673] (2006)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Liquid crystals

Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.

Links