C

n=sqrt(1+1.17365704/(1-0.00577031797/pow(x,2))+0.588992398/(1-0.0200401678/pow(x,2))+0.978014394/(1-95.4873482/pow(x,2)))

Python

n=(1+1.17365704/(1-0.00577031797/x**2)+0.588992398/(1-0.0200401678/x**2)+0.978014394/(1-95.4873482/x**2))**.5

Fortran

n=SQRT(1+1.17365704/(1-0.00577031797/x**2)+0.588992398/(1-0.0200401678/x**2)+0.978014394/(1-95.4873482/x**2))

MATLAB

n=sqrt(1+1.17365704./(1-0.00577031797./x.^2)+0.588992398./(1-0.0200401678./x.^2)+0.978014394./(1-95.4873482./x.^2))

LaTeX

n^2-1=\frac{1.17365704λ^2}{λ^2-0.00577031797}+\frac{0.588992398λ^2}{λ^2-0.0200401678}+\frac{0.978014394λ^2}{λ^2-95.4873482}