n=sqrt(3.11724527-0.00977958678*pow(x,2)+0.0431752564*pow(x,-2)+0.00252279577*pow(x,-4)-0.00011739974*pow(x,-6)+2.07881157e-05*pow(x,-8))

Python

n=(3.11724527-0.00977958678*x**2+0.0431752564*x**-2+0.00252279577*x**-4-0.00011739974*x**-6+2.07881157e-05*x**-8)**.5

Fortran

n=SQRT(3.11724527-0.00977958678*x**2+0.0431752564*x**-2+0.00252279577*x**-4-0.00011739974*x**-6+2.07881157e-05*x**-8)

MATLAB

n=sqrt(3.11724527-0.00977958678.*x.^2+0.0431752564.*x.^-2+0.00252279577.*x.^-4-0.00011739974.*x.^-6+2.07881157e-05.*x.^-8)

LaTeX

n^2=3.11724527-0.00977958678λ^{2}+0.0431752564λ^{-2}+0.00252279577λ^{-4}-0.00011739974λ^{-6}+2.07881157\text{×}10^{-05}λ^{-8}