n2 Explorer: Yb:KY(WO4)2 (Ytterbium doped potassium yttrium tungstate, Yb:KYW)

Selivanov et al. 2006: n2(α)
Selivanov et al. 2006: n2(β)
Selivanov et al. 2006: n2(γ)

LogX   LogY   eV

Details

Selivanov et al. 2006: n2(α)
Selivanov et al. 2006: n2(β)
Selivanov et al. 2006: n2(γ)

Reference

Comments

Data




Conditions




Additional information