n2 Explorer: SrNb2O6-BaNb2O6 (Strontium-barium niobate, SBN)
Jansonas et al. 2022: SBN61; (o)
LogX
LogY
eV
Details
Reference
Comments
Data
Conditions
Additional information
About Strontium-barium niobate
Other names and variations:
- SrxBa(1-x)Nb2O6
- SBN